Durobord is India's No 1 blockboard due its superior quality and durability. Durobord blockboards are double pressed to ensure a smooth wrap free surface and is also free from corrugation and gaps, establishing itself as the finest quality blockboard in India. Durobord is dimensionally stable and made from kiln dried seasoned timber that can resist termites and other wood-destroying organisms. Available in both BWP and MR grade, conforms to IS:1659 (2004)

With 100% Lifetime Guarantee
  • Carpenter Friendly

    Durobord has the advantage of being carpenter friendly, light in weight, easy on tools and can hold screws and nails firmly.

  • Durable Timber

    Durobord is made with the finest quality of AAA grade and kiln seasoned Pine timber filler, hardwood cross core and superior grade face veneer. This unique combination of fine raw material ensures lifelong durability.

  • Smooth Surface

    Each sheet of Durobord is double pressed and calibrated for a smooth, warp free surface that is free from corrugation and gaps.

  • Termite Treatment

    Durobord has an extremely high vertical load bearing strength making it ideal for all vertical applications such as cupboard shutters.

Technical Specifications

Conforming to IS : 1659 (2004)

Prescribed Test Values for Conformity Observed Value
Moisture Content (%) 5 - 15 10 - 5
Modulus of Elasticity (N/mm2) 5000 5500 - 5300
Modulus of Rapture (N/mm2) 50 55 - 52
Water Absorption (%) <5 <5
Screw Holding Strength(Kgs) 80 100
Nail Holding Strength(Kgs) 50 55
Squareness Test (%) 0.2 0.4 - 0.6
Edge Straightness Test (%) 0.2 0.6 - 0.8
Water Resistance Test No delamination after 72 hours in
boiling water at 100°C ± 2°C temperature
Conforms
Prescribed Test Values for Conformity Observed Value
Moisture Content (%) 5 - 15 10 - 5
Modulus of Elasticity (N/mm2) 5000 5500 - 5300
Modulus of Rapture (N/mm2) 50 55 - 52
Water Absorption (%) <5 <5
Screw Holding Strength(Kgs) 80 100
Nail Holding Strength(Kgs) 50 55
Squareness Test (%) 0.2 0.4 - 0.6
Edge Straightness Test (%) 0.2 0.6 - 0.8
Water Resistance Test No delamination after 72 hours in
boiling water at 100°C ± 2°C temperature